Tsarin shiri na polyamide adhesives
Bar sako
Shirye-shiryen Dimeric Linoleic Acid: Linoleic acid, yumbu, lithium carbonate, da ruwa an kara su zuwa wani reactor kuma an motsa shi a matsa lamba na 0.8-1.2 MPa. An ɗaga zafin jiki zuwa digiri 230 kuma ya amsa tsawon sa'o'i 5. An sanyaya cakuda zuwa digiri 100, kuma an ƙara 1.92 g na phosphoric acid aqueous bayani. Sannan an rage matsa lamba zuwa 0.3-0.5 MPa, kuma an ɗaga zafin jiki zuwa digiri 150 na awa 1. A ƙarshe, an saukar da zafin jiki zuwa digiri 100, kuma an tace cakuda yayin zafi don cire mai kara kuzari. Fatty acids mara saturated fatty acids sannan an kwashe su a ƙarƙashin babban injin (6.7-10.7 Pa) a digiri 220-225 don samun tsaftar linoleic acid mai girma{20}.
Shiri na Polyamide Hot Melt Adhesive: A ƙarƙashin kariya ta nitrogen, an ƙara cakuda ethylenediamine da hexamethylenediamine a hankali a hankali yayin motsawa da dumama cakuda zuwa digiri 130. A wannan gaba, ana sarrafa zafin jiki a digiri 140-150. Bayan an gama ƙarawa, ana ƙara yawan zafin jiki zuwa digiri 205-220 kuma ana ci gaba da amsawa har sai abin da ke cikin ruwa na samfurin ya kusanci ƙimar ka'idar. Sa'an nan, an rage matsa lamba, kuma ana ci gaba da amsawa don wani sa'a a 1.3-2.7 kPa da 220-230 digiri. A ƙarshe, ana ɗaukar samfurin don tantance ƙimar aminin. Idan ya hadu da fihirisar (kimanin 10), samfurin na iya sanyaya da fitarwa. Matsayin laushi na mannen narkewar zafi ya bambanta dangane da adadin dilinoleic acid, sebacic acid, ethylenediamine, da hexamethylenediamine da aka yi amfani da su.